A286 Iron-Base Superalloy Speeds and Feeds (Milling, Drilling, Turning)

    Carbide end mills in A286 Iron-Base Superalloy: 100–300 SFM. Also called UNS S66286, AMS 5737. Chart row used: “Monel & High Nickel Steel” (Aged).

    Starting point: carbide end mills

    RPM and IPM use the low end of the published range (100 SFM and the lowest chip load for each diameter range). RPM = SFM × 12 ÷ (π × D); IPM = RPM × flutes × chip load.

    A286 Iron-Base Superalloy — inch end mills
    DiameterChip load (in/tooth)RPMIPM · 2 fluteIPM · 3 flute
    1/8".00033,0561.82.8
    1/4".00031,5280.91.4
    3/8".00061,0191.21.8
    1/2".00107641.52.3
    3/4".00155091.52.3
    1".00203821.52.3
    A286 Iron-Base Superalloy — metric end mills (inch chip-load range the size falls in)
    DiameterChip load (in/tooth)RPMIPM · 2 fluteIPM · 3 flute
    3 mm.00033,2341.92.9
    6 mm.00031,6171.01.5
    10 mm.00109701.92.9
    12 mm.00108091.62.4
    16 mm.00156061.82.7
    20 mm.00204851.92.9
    Full published chip-load ranges
    • 1/32-1/8": .0003–.0006"
    • 1/8-1/4": .0003–.0010"
    • 1/4-3/8": .0006–.0015"
    • 3/8-1/2": .0010–.0020"
    • 1/2-3/4": .0015–.0030"
    • 3/4-1": .0020–.0040"

    Calculator — prefilled for A286 Iron-Base Superalloy

    Results for Milling

    Spindle RPM
    764
    Feed
    3.1 IPM
    Chip load
    0.0009 in
    MRR
    0.11 in³/min
    Power
    — HP
    Torque
    — lbf·ft
    Programmed fz
    0.0010 in
    Actual SFM
    100
    Spindle use
    6%
    • Pick a material in the library below to estimate spindle power and torque.

    Material library

    Tool & coating guidance

    Grade, edge geometry and coating determine usable cutting data. Sharp polished edges can suit nonferrous work; substrate and geometry still govern. Coated vs uncoated carbide changes turning data only; no coating speed multiplier is inferred.

    Tool & cut parameters

    Manual values
    Chip thinning & cutter body
    %
    Radial factor ×1.09Angle factor ×1.00Programmed fz 0.0010 inMax chip hex 0.0009 in

    Fixed-angle peripheral estimate: hex = fz × radial factor × sin(KAPR). No radial correction at ≥50% engagement. Not a centered face-milling or ball-nose model. Sandvik geometry reference

    Insert styles, guidelines & formulas

    RPM = (SFM × 12) / (π × D) | Feed = RPM × programmed fz × effective zc | MRR = WOC × DOC × feed | HP = Kp × C × MRR × 1.1 ÷ 0.8 (Machinery's Handbook)

    Square (SEMT/SNMG)
    General purpose, 90° lead angle
    Round (RPMW/RCKT)
    Ramping, 3D contouring, high feed
    Triangular (TPMX)
    Light cuts, finishing
    Octagonal (ONMU)
    Face milling; HFM suitability is body-specific

    Milling Guidelines

    • Start at 70% of max SFM, increase gradually
    • Chip load too low → rubbing & heat buildup
    • Use climb milling when machine rigidity allows
    • Radial engagement >50% → reduce feed per tooth
    • Round inserts: best for ramp-in and 3D surfaces
    Open in the full calculator workspace

    Speeds by tool material

    Published starting ranges for A286 Iron-Base Superalloy by operation and tool material. Rows marked * are estimates.

    A286 Iron-Base Superalloy — speeds by tool material
    OperationToolSFMFeedSource row
    millingSolid carbide end mill100–3000.0010–0.0020 in/toothLakeshore Carbide · Monel & High Nickel Steel
    millingUncoated carbide (H13A)120–1450.0040–0.0080 in hexSandvik milling (large engagement) · CMC 20.12 Iron-base superalloy, aged
    millingCoated carbide (GC1030)120–1500.0040–0.0080 in hexSandvik milling (large engagement) · CMC 20.12 Iron-base superalloy, aged
    turningUncoated carbide (H13A)130–1950.0040–0.0200 in/revSandvik turning · CMC 20.12 Iron-base superalloy, aged
    turningCoated carbide (GC1115)155–3150.0040–0.0200 in/revSandvik turning · CMC 20.12 Iron-base superalloy, aged

    Machinist tips

    Chip thinning
    At light radial engagement (under half the cutter diameter) the real chip is thinner than the feed per tooth. Raise the feed to keep the chip at the chart value, or the tool rubs and wears.
    Climb vs conventional
    On a rigid CNC, climb mill so each tooth starts thick and exits thin. Use conventional milling on machines with backlash or on hard scale skins.
    Heat is the enemy
    Use high-pressure coolant, keep engagement consistent, and stay at the low end of the speed range.

    Common questions

    What SFM should I use for A286 Iron-Base Superalloy?
    Lakeshore Carbide – General Purpose End Mill Speeds & Feeds lists 100–300 SFM for carbide end mills in the "Monel & High Nickel Steel" row. Start at the low end and adjust for your machine.
    What chip load for a 1/2" end mill in A286 Iron-Base Superalloy?
    The published range for 3/8–1/2" carbide end mills is .0010–.0020" per tooth. At 100 SFM a 3-flute 1/2" end mill runs about 764 RPM and 2.3 IPM.
    Are these values for HSS tools, drilling or turning?
    The end mill chart covers carbide end mills. The "Speeds by tool material" table adds published HSS, turning-insert and drilling rows for A286 Iron-Base Superalloy where a source lists them (LittleMachineShop, Sandvik Coromant).
    A286 · Solution Treated speeds and feedsTitanium Grade 1 (CP) speeds and feedsTitanium Grade 2 (CP) speeds and feeds

    Sources

    Starting values only. Adjust for rigidity, tool manufacturer data and machine.

    Free for machinists & programmers

    Put your skills on a free talent profile

    Machines, controls, certs and saved calculations in one profile shops can find.

    Create free profile
    For your shop

    Bring shift handoffs to your shop

    Stop losing job status between shifts. Every station's notes, counts and issues, handed off cleanly.

    See shift handoffs